Features of S355J2N/Is 2062 E350C
S355J2 (without the “N”):
- S355J2 is a European standard structural steel grade (EN 10025-2) known for its good strength and weldability.
- It typically has a minimum yield strength of 355 MPa and is often used in construction and engineering projects.
IS 2062 E350 (without the “C”):
- IS 2062 E350 is an Indian standard for hot-rolled structural steel.
- It usually has a minimum yield strength of 250 MPa.
>> What is S355J2N / IS 2062 E350C?
S355J2N:
- S355J2N is not a standard grade of steel. It appears to be a partial designation. The “S355” typically refers to a structural steel grade, and the “J2” is a specific subgrade within the S355 series.
- S355 is a non-alloy structural steel grade according to the European standard EN 10025-2. It is commonly used in construction and engineering applications.
- The “J2” indicates that the steel has a minimum impact energy of 27 J at -20°C. This means it is suitable for low-temperature applications.
- The “N” likely signifies that the steel is normalized, which is a heat treatment process to improve its properties.
IS 2062 E350C:
- IS 2062 is an Indian standard for hot-rolled medium and high tensile structural steel. It is widely used in various construction and structural applications in India.
- E350C is a specific grade within the IS 2062 standard. The “E” stands for E Series, which signifies that it is a high-strength, medium-carbon steel. The “350” indicates the minimum yield strength of the steel in megapascals (MPa), which is 350 MPa.
- The “C” may signify that it is a controlled-rolled steel, which implies that it has controlled processing to achieve desired mechanical properties.
>> Differnce Between S355J2N And IS 2062 E350C
“S355J2N” and “IS 2062 E350C” are not direct equivalents, but they are both related to steel grades used in structural applications. Here’s a comparison between the two:
Origin and Standards:
- “S355J2N” typically refers to a steel grade that follows European standards, particularly EN 10025-2. It is widely used in Europe and internationally.
- “IS 2062 E350C” is an Indian standard for structural steel.
Grade Specifications:
- S355J2N is a subgrade of the S355 steel series, indicating its specific properties. “S355” indicates the minimum yield strength of 355 MPa.
- IS 2062 E350C is part of the IS 2062 steel series and designates a structural steel with a minimum yield strength of 350 MPa.
Heat Treatment:
- S355J2N doesn’t specify a particular heat treatment, but it is often used as normalized steel in its delivery condition.
- IS 2062 E350C may be controlled-rolled, thermomechanically rolled, or normalized, depending on the manufacturer’s specifications.
Applications:
- S355J2N is used in a wide range of international structural applications, including building construction, bridges, and machinery.
- IS 2062 E350C is commonly used in structural and construction applications in India and may have regional variations in usage.
Geographical Usage:
- S355J2N is more commonly used in European and international construction projects.
- IS 2062 E350C is predominantly used in India and neighboring regions.
Manufacturers and Suppliers:
- S355J2N steel can be sourced from various international manufacturers and suppliers.
- IS 2062 E350C is typically available from Indian steel manufacturers and suppliers.
>> Equivalent Grade of S355J2N / IS 2062 E350C
The equivalent grade of “S355J2N” and “IS 2062 E350C” will depend on the specific standards and requirements for your project. Both of these steel grades are used in structural and construction applications, but they are associated with different standards (European and Indian, respectively).
EQUIVALENT GRADE OF S355J2 PLATE
EN 10025-2 | Germany DIN 17100 | UNI | JIS | GOST | ||
S355J2 | 1.0577 | St 52.3 | 1.0570 | Fe510D | SS490YA | 17G1S |
>> Specifications of S355J2N / Is 2062 E350C
“S355J2N” and “IS 2062 E350C” are steel grades used in structural and construction applications, but specific specifications may vary depending on regional and national standards and project requirements. Below, I’ll provide a general overview of the specifications for these grades:
S355J2N (per European standard EN 10025-2):
- Minimum Yield Strength: 355 MPa
- Tensile Strength: 450-680 MPa
- Elongation: 20% (at 20°C)
- Impact Test: 27 Joules at -20°C
- Chemical Composition: The precise chemical composition may vary, but typically, S355J2N is a non-alloy structural steel with elements such as carbon, manganese, silicon, sulfur, phosphorus, and trace amounts of other elements. It may contain micro-alloying elements for enhanced properties.
IS 2062 E350C (per Indian standard IS 2062):
- Minimum Yield Strength: 350 MPa
- Tensile Strength: 490-650 MPa
- Elongation: Varies depending on the thickness of the material.
- Chemical Composition: The chemical composition of IS 2062 E350C typically includes carbon, manganese, sulfur, phosphorus, silicon, and sometimes other alloying elements based on the manufacturer’s specifications.
SPECIFICATION
Item | S355J2 – Offshore & Structural Steel Plate |
Thickness | 5mm-150mm |
Width | 1000mm-4500mm |
Length | 3000mm-18000mm or as custom’s request |
Material | En 10025-2 Steel Plate, S355J2 Steel Plate |
Technique | hot rolled |
Standard | EN 10025-2:2004 |
>> Chemical Composition of S355J2N / Is 2062 E35
S355J2N (per European standard EN 10025-2):
- Carbon (C): Typically, the carbon content is less than 0.22%.
- Silicon (Si): Usually, the silicon content is less than 0.55%.
- Manganese (Mn): Typically, the manganese content ranges from 1.60% to 1.80%.
- Phosphorus (P): The maximum phosphorus content is typically 0.035%.
- Sulfur (S): The maximum sulfur content is typically 0.035%.
- Other alloying elements: There may be small amounts of other alloying elements, such as traces of niobium, vanadium, or titanium, depending on specific requirements.
IS 2062 E350C (per Indian standard IS 2062):
- Carbon (C): Generally, the carbon content is less than 0.25%.
- Silicon (Si): Typically, the silicon content is less than 0.40%.
- Manganese (Mn): The manganese content is usually in the range of 1.50% to 1.80%.
- Phosphorus (P): The maximum phosphorus content is typically 0.040%.
- Sulfur (S): The maximum sulfur content is typically 0.040%.
- Other alloying elements: Similar to S355J2N, there may be small amounts of other alloying elements, depending on the manufacturer’s specifications and the specific project requirements.
CHEMICAL COMPOSITION OF S355J2 PLATE
Grade | C | Mn | Si | P | S | Cu | CEV |
S355J2 | 0.22 max. | 1.6 max. | 0.55 max. | 0.03 max. | 0.03 max. | 0.55 max. | 0.47 max. |
>> Mechanical Properties of S355J2N / Is 2062 E350C
S355J2N (per European standard EN 10025-2):
- Minimum Yield Strength: 355 MPa
- Tensile Strength: 450-680 MPa
- Elongation: 20% (at 20°C)
- Impact Test: 27 Joules at -20°C
IS 2062 E350C (per Indian standard IS 2062):
- Minimum Yield Strength: 350 MPa
- Tensile Strength: 490-650 MPa
- Elongation: Varies depending on the thickness of the material.
MECHANICAL PROPERTIES OF ASTM A588 CORTEN B PLATES & SHEETS
Minimum yield strength Reh MPa |
Tensile strength Rm MPa |
Minimum elongation – A Lo = 5,65 * √So (%) |
Notch impact test |
|||||||||||
Steel grade |
Nominal thickness mm |
Nominal thickness mm |
Nominal thickness mm |
Temperature |
Min. absorbed energy |
|||||||||
≤16 |
>16 ≤40 |
>40 ≤63 |
>63 ≤80 |
>80 ≤100 |
>100 ≤125 |
>3 ≤100 |
>100 ≤125 |
>3 ≤40 |
>40 ≤63 |
>63 ≤100 |
>100 ≤125 |
°C |
J |
|
S355J2 |
355 |
345 |
335 |
325 |
315 |
295 |
470-630 |
450-600 |
22 |
21 |
20 |
18 |
-20 |
27 |
PEOPLE ALSO SEARCHED FOR S355J2 PLATE
Plate Size available Ex-Stock of SAILMA 550HI, SAILMA E550, IS 2062 E550
1mm | 2mm | 3mm | 4mm | 6mm | 8mm | 10mm | 12mm | 14mm | 16mm | 20mm |
25mm | 30mm | 32mm | 36mm | 40mm | 45mm | 50mm | 63mm | 70mm | 72mm | 75mm |
80mm | 90mm | 100mm | 110mm | 130mm | 150mm | 170mm | 180mm | 200mm | 230mm | 270mm |
300mm |